+86-13915203580

High-pressure Hydraulic Cylinder Barrel – Exported to European market

Home / News / Company News / High-pressure Hydraulic Cylinder Barrel – Exported to European market

High-pressure Hydraulic Cylinder Barrel – Exported to European market

High-pressure hydraulic cylinder barrel is a critical component that performs core functions in hydraulic transmission systems. Its structural design and manufacturing precision directly determine whether the entire hydraulic system can operate stably and efficiently, playing a vital role in the overall performance of the system. Below are the key features of our company's high-pressure cylinder bodies:


1.High-strength Materials: We employ high-strength materials that meet stringent industrial standards for manufacturing cylinder bodies, enhancing the overall structural strength from the raw material perspective while significantly improving wear resistance on operational surfaces to extend service life.


2.Precision Machining: The stepped structure manufactured using high-precision CNC equipment enables precise dynamic fit between the cylinder body and its mating components, effectively reducing friction losses during operation and ensuring long-term efficient and stable performance of the entire hydraulic system.


3.Buffering Device: The buffering device integrated into the cylinder body operates on the fundamental principle of fluid throttling, enabling smooth deceleration when the piston reaches the end of its stroke, effectively mitigating impact forces at the stroke endpoint and reducing operational impacts and noise during equipment operation.

 
4. Exhaust Valve: In our high-pressure cylinder units, the exhaust valve is typically positioned at the highest point of the cylinder barrel, ensuring timely discharge of accumulated gas to prevent cavitation damage to the cylinder walls and maintain smooth cylinder movement.

Material:ASME SA350 LF2 Class 1
EN 10222-4 P355NH (TRgOmm) or P355QH1 (TR≥70mm)
5.1 Impact test CHARPY-V EN-lSO 148-1 at -46oC or lower.

T.SRm(Mpa)

Y.SRp0.2(Mpa)

A%

Z%

S.D

485–655

≥315

≥22

≥30