+86-13915203580

Certification

Home / Certification
Quality System
Founded in 2004, Jiangyin Xinyu Forging Co., Ltd. is a growing forging manufacturer that offers a wide range of mechanical forgings for valves and oil recovery equipment.

We specialise in the production of open die forgings, closed die forgings and seamless rings, and are capable of producing any complex shapes up to 20 ft OD and 40,000 lbs, including raw forgings or finish machined products.
  1. ISO 9001
  2. ISO 14001 EMS
  3. ISO 45001 OHS
  4. API Monogram 20B 2024
  5. PED
  6. UKCA
  7. ISO 50001 EnMS
Test Laboratory
Quality control capability
All of our forgings are 99.99% UT to ASTM, API or customer specified specifications. Chemical verification is 99.99% per heat. Destructive testing is performed on each hot lot to verify mechanical compliance.
  • Chemistry Confirmation

  • Tensile Testing

  • Microstructure Analysis

  • MPI (ASNT level II)

  • Hardness (Rockwell C and Brinell)

  • Charpy Impact testing (-150 degree C)

  • UT (ASNT level II)

  • LPI (ASNT level II)